Please use the table below to select the correct micro etchant for your superalloy.
Name of the Alloy: | Etchant to Use: |
A286 | Fry’s |
AerMet 100, 310, 340 | Fry’s |
Inconel 625, MP35N, Hastelloy C-276 | Adler’s |
Inconel 718 | Kalling’s 2 |
Inconel 600, 713, 901, X750 | Superalloy etch |
Hastelloy X | Superalloy etch |
Jethete | Fry’s |
Themo-Span | Fry’s or Kalling’s 2 |
Monel, Kovar | Fry’s |
Waspaloy | Superalloy Etch |
Others | See this list |