Superalloy Etch is a modified and stronger version of the standard Kalling’s no. 2 reagent. It is specifically engineered for high corrosion-resistant superalloys like Waspaloy, C263, Hastelloy X, Inconel 600, 713, and 901. Made with reagent-grade chemicals to ensure quality and reliability.
User Instructions:
- Mirror-polish the superalloy sample with diamond slurry or alumina (1 µm or finer) before etching. Avoid using colloidal silica, as the residue might react with the etchant.
- The metal surface must be etched immediately after polishing, cleaning, and drying. Otherwise, these highly corrosion-resistant alloys will passivate.
- Use this product under a fume hood. Immerse or swab the polished surface for a few seconds to a minute.
- Rinse the sample with water to stop the reaction once the desired outcome is achieved.
Packaging:
Nalgene® Leakproof Bottle, HDPE.
Additional information
| Weight | 0.8 lbs |
|---|---|
| Dimensions | 4.4 × 2.7 × 6.5 in |
You may also like…
-
Now serving US & Canada.🇺🇸🇨🇦
-
All prices are in $USD.
-
Overnight and UPS collect available.
-
Commercial shipping address required.