Superalloy Etch (Mod. Kalling’s), 250 mL

$73.45

Description

Superalloy Etch is a modified and stronger version of the standard Kalling’s no. 2 reagent. It is specifically engineered for high corrosion-resistant superalloys like Waspaloy, C263, Hastelloy X, Inconel 600, 713, and 901. Made with reagent-grade chemicals to ensure quality and reliability.

User Instructions:

  • Mirror-polish the superalloy sample with diamond slurry or alumina (1 µm or finer) before etching. Avoid using colloidal silica, as the residue might react with the etchant.
  • The metal surface must be etched immediately after polishing, cleaning, and drying. Otherwise, these highly corrosion-resistant alloys will passivate.
  • Use this product under a fume hood. Immerse or swab the polished surface for a few seconds to a minute.
  • Rinse the sample with water to stop the reaction once the desired outcome is achieved.

Packaging:

Nalgene® Leakproof Bottle, HDPE.

Waspaloy etched with Superalloy Etch

Additional information

Weight 0.8 lbs
Dimensions 4.4 × 2.7 × 6.5 in
  • Now serving US & Canada.🇺🇸🇨🇦

  • All prices are in $USD.

  • Overnight and UPS collect available.

  • Commercial shipping address required.