“Nital Etch, 5%, 500 mL” has been added to your cart. View cart
“Ferric Chloride Etchant, 250 mL” has been added to your cart. View cart
“Keller’s Reagent, 250 mL” has been added to your cart. View cart
Superalloy Etch (Mod. Kalling’s), 250 mL
SKU: 155
Categories: METALLOGRAPHIC ETCHANTS, SUPERALLOY ETCHANTS
$73.45
Description
Superalloy Etch is a modified and stronger version of the standard Kalling’s no. 2 reagent. It is specifically engineered for high corrosion-resistant superalloys like Waspaloy, C263, Hastelloy X, Inconel 600, 713, and 901. Made with reagent-grade chemicals to ensure quality and reliability.
User Instructions:
- Mirror-polish the superalloy sample with diamond slurry or alumina (1 µm or finer) before etching. Avoid using colloidal silica, as the residue might react with the etchant.
- The metal surface must be etched immediately after polishing, cleaning, and drying. Otherwise, these highly corrosion-resistant alloys will passivate.
- Use this product under a fume hood. Immerse or swab the polished surface for a few seconds to a minute.
- Rinse the sample with water to stop the reaction once the desired outcome is achieved.
Packaging:
Nalgene® Leakproof Bottle, HDPE.
Additional information
| Weight | 0.8 lbs |
|---|---|
| Dimensions | 4.4 × 2.7 × 6.5 in |
You may also like…
-
Now serving US & Canada.🇺🇸🇨🇦
-
All prices are in $USD.
-
Overnight and UPS collect available.
-